20deg celcius 30000N CAM V8 bron data Tensile Strengt: ansys eneneering datasources Structural Steel(metal): 5,6575e8 Pa / -2,5163e9 Pa 2,5E+08 Pa Tensile Yield Strength 4,6E+08 Pa Tensile Ultimate Strength 7850 kg*m-3 Titanium Alloy(metal): 5,6506e8 Pa / -2,5053e9 Pa 9,3E+08 Pa Tensile Yield Strength 1,07E+09 Pa Tensile Ultimate Strength 4620 kg*m-3 Alumininum Alloy(metal): 5,6463e8 Pa / -2,5128e9 Pa 2,8E+08 Pa Tensile Yield Strength 3,1E+08 Pa Tensile Ultimate Strength 2770 kg*m-3 Stainless Steel(metal): 5,6352e8 Pa / -2,5155e9 Pa 2,07E+08 Pa Tensile Yield Strength 5,86E+08 Pa Tensile Ultimate Strength 7750 kg*m-3 Polyethylene(plastic): 5,589e8 Pa / -2,4662e9 Pa 2,5E+07Pa Tensile Yield Strength 3,3E+07Pa Tensile Ultimate Strength 950 kg*m-3 Plastic, ABS(plastic): 5,6102e8 Pa/ -2,4773e9 Pa 2,772E+07 Pa Tensile Yield Strength 3,813E+07 Pa Tensile Ultimate Strength 1030 kg*m-3 Wood, oak(organic): 5,646e8 Pa / -2,4997e9 Pa ~4,5E+07 Pa Tensile Yield Strength ~1,45E+08 Pa Tensile Ultimate Strength 925,7 kg*m-3 Geen één heeft genoeg kracht, data sim output is overal bijna gelijk. Niet nodig om de heletijd herhalen. ------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------ CAM V9 : 4,8422e8 Pa / -4,7053e8 Pa --> 4,8422e8 Pa dus mogelijke materiaalen: Titanium Alloy Stainless Steel (buigt wel permanent) Structural Steel (buigt ook permanent) dus: Titanium Alloy