44
|
20deg celcius
30000N
CAM V8
bron data Tensile Strengt: ansys eneneering datasources
Structural Steel(metal): 5,6575e8 Pa / -2,5163e9 Pa
2,5E+08 Pa Tensile Yield Strength
4,6E+08 Pa Tensile Ultimate Strength
7850 kg*m-3
Titanium Alloy(metal): 5,6506e8 Pa / -2,5053e9 Pa
9,3E+08 Pa Tensile Yield Strength
1,07E+09 Pa Tensile Ultimate Strength
4620 kg*m-3
Alumininum Alloy(metal): 5,6463e8 Pa / -2,5128e9 Pa
2,8E+08 Pa Tensile Yield Strength
3,1E+08 Pa Tensile Ultimate Strength
2770 kg*m-3
Stainless Steel(metal): 5,6352e8 Pa / -2,5155e9 Pa
2,07E+08 Pa Tensile Yield Strength
5,86E+08 Pa Tensile Ultimate Strength
7750 kg*m-3
Polyethylene(plastic): 5,589e8 Pa / -2,4662e9 Pa
2,5E+07Pa Tensile Yield Strength
3,3E+07Pa Tensile Ultimate Strength
950 kg*m-3
Plastic, ABS(plastic): 5,6102e8 Pa/ -2,4773e9 Pa
2,772E+07 Pa Tensile Yield Strength
3,813E+07 Pa Tensile Ultimate Strength
1030 kg*m-3
Wood, oak(organic): 5,646e8 Pa / -2,4997e9 Pa
~4,5E+07 Pa Tensile Yield Strength
~1,45E+08 Pa Tensile Ultimate Strength
925,7 kg*m-3
Geen één heeft genoeg kracht, data sim output is overal bijna gelijk. Niet nodig om de heletijd herhalen.
------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------
CAM V9 : 4,8422e8 Pa / -4,7053e8 Pa --> 4,8422e8 Pa
dus mogelijke materiaalen:
Titanium Alloy
Stainless Steel (buigt wel permanent)
Structural Steel (buigt ook permanent)
dus: Titanium Alloy
|